Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.99 J/cm @Temperature 23.0 °C |
7.47 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Noble Polymers Regis™ 155120 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Izod Impact, Notched | 3.99 J/cm @Thickness 6.35 mm |
7.47 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chi Mei Polylac® PA-709S ABS - Extrusion Super Impact Extrusion |