Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.04 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
5.70 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8003 A1 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Comp.. |
|||
Izod Impact, Notched | 3.04 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
5.70 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS E Availability: North AmericaForms: PelletsFeatures: High ViscosityProcessing Method: Blow Molding and ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 3.04 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
5.70 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS HH BK MB Availability: North AmericaForms: PelletsFeatures: High Gloss and High Heat ResistanceAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 3.04 J/cm @Temperature 23.0 °C |
5.70 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 307E0V16310 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |