Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm |
4.01 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Trilac® ABS-HH2500 Super High Heat ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
4.01 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
notch |
Kraton® G1651 + PC blend (5/95) Blending KRATON D and G polymers with PC significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature -29.0 °C |
4.01 ft-lb/in @Temperature -20.2 °F |
3.2 mm (0.125 in) notch |
Kraton® G1657 + PA-6,6 blend (16/4/80) Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 23.0 °C |
4.01 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 360E3V45508 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 23.0 °C |
4.01 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 371A2R30008 Cellulose Acetate Propionate, Natural, Trsp Applications:Consumer-Personal CareToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, c.. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
4.01 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers Centrex® 825 Sheet Extrusion Grade Centrex 825 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it .. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
4.01 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers Centrex® 925 Injection Molding Grade Centrex 925 resin is a soft-flow, high-gloss, molding grade of Polycarbonate / ASA (acrylonitrile-styrene-acrylate) blend. It is an injection molding grade with a good balance of physical properties.. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
4.01 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers NPP25-0604 Impact Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |