Polymer Property : Izod Impact, Notched = 3.99 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.13 J/cm

@Temperature 23.0 °C
3.99 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycolac® MG34LGHF ABS
Low gloss, high flow ABS for unpainted interior applications.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 2.13 J/cm

@Temperature 23.0 °C
3.99 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycolac® X37 ABS
ABS, injection moulding, high heat grade.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 2.13 J/cm

@Temperature 23.0 °C
3.99 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycolac® Z48 ABS
Automotive. Very high heat resistance with medium impact and good strength properties.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 2.13 J/cm

@Temperature -30.0 °C
3.99 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® EM3110R PC
Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. Internal mold release.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 2.13 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
3.99 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® EM3110R PC
Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. Internal mold release.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 2.13 J/cm

@Temperature 23.0 °C
3.99 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl PX1127 PPE+PS
Automotive electrical applications. 250F (120C) HDT.This data was supplied by SABIC-IP for the Americas region.