Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.90 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M4805 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5705 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 6.86 J/cm @Temperature 23.0 °C |
12.9 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
PolyMirae Moplen EP300C Sheet and Thermoforming Grade Polypropylene Moplen EP300C is the polypropylene blockpolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300C is a block copolymer particularly suitable for sheet and t.. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-500-CU00 Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 6.90 J/cm @Temperature 23.0 °C |
12.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Europe-Africa-Middle East) Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors.This data was supplied b.. |
|||
Izod Impact, Notched | >= 6.86 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 12.9 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY SC1004A PC Description: Injection Molding, PC, General Purpose, High Toughness, Chemical resistance, High Impact (at Low Temperature)Application: Mobile Phone HousingCAS: 103598-77-2 and 143106-82-5Information.. |
|||
Izod Impact, Notched | 6.86 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® CF-1051 PC, Unreinforced High Impact High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.86 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® CF-1070 PC, Unreinforced High Impact High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.86 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NH-1021 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.86 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® CF-1051 PC, Unreinforced High Impact High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.86 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® CF-1070 PC, Unreinforced High Impact High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M4820 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 6.86 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NH-1021 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | >= 6.86 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 12.9 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY NS5000C PC/ABS, High Impact Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High ImpactApplication: Automotive (Interior)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 6.86 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 12.9 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY SC1004ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Good Coloring, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical.. |