Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.10 J/cm @Temperature 23.0 °C |
11.4 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by .. |
|||
Izod Impact, Notched | 6.09 J/cm @Temperature 23.0 °C |
11.4 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Noble Polymers Regis™ 190108 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Izod Impact, Notched | 6.08 J/cm @Temperature -20.0 °C |
11.4 ft-lb/in @Temperature -4.00 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® 1101 PBT+PC (Asia Pacific) Unreinforced, opaque polycarbonate/polyester alloy. Excellent low temperature impact plus chemical resistance to automotive fluid.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 6.08 J/cm @Thickness 3.17 mm |
11.4 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HP-1000H PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.08 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
11.4 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1098 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.08 J/cm @Thickness 3.17 mm |
11.4 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HP-1000H PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.08 J/cm @Thickness 3.17 mm |
11.4 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HP-1000P PC/ABS, Unreinforced High flow material that can be used in the exterior material of mobile phone, wheel cap, rice cooker, electric iron etc. as well as refrigerator door handle and panelInformation provided by Samsung .. |
|||
Izod Impact, Notched | 6.08 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
11.4 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1098 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.08 J/cm @Thickness 3.17 mm |
11.4 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HP-1000P PC/ABS, Unreinforced High flow material that can be used in the exterior material of mobile phone, wheel cap, rice cooker, electric iron etc. as well as refrigerator door handle and panelInformation provided by Samsung .. |