Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.50 J/cm @Temperature 23.0 °C |
10.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Izod Impact, Notched | 5.50 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
10.3 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH950-602 Low-temperature Resistant & Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surface, high glossApplications:ControllerPlug, socketShell of ammeterSmall hou.. |
|||
Izod Impact, Notched | 5.49 J/cm @Thickness 3.17 mm |
10.3 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® AE-2130 PC/PET, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.49 J/cm @Thickness 3.17 mm |
10.3 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® AE-2130 PC/PET, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature 23.0 °C |
10.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® V3802 PBT + PC + PET (Asia Pacific) PBT + PC + PET, Mold Release, Flame retardant, Impact Modified, OpaqueThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature 23.0 °C |
10.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND 4500 V0 HF Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, chlorine and bromine free, good light resistance, excellent mechanical properties, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature 23.0 °C |
10.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND 4501 V0/D Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, PBDE and antimony free, with halogens, high impact resistance, very high thermal resistance, high gloss, good processabilityInformation provided by Cossa Poli.. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature 0.000 °C |
10.3 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTABLEND 7500 V0 HF Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, chlorine and bromine free, good light resistance, good thermal and mechanical properties, excellent processabilityInformation provided by Cossa Polimeri S.r.l.. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature 23.0 °C |
10.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND 8500 V0 HF Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, chlorine and bromine free, good light resistance, good thermal and mechanical properties, excellent processabilityInformation provided by Cossa Polimeri S.r.l.. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature 23.0 °C |
10.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND PSA 8500 V0 Flame Retardant PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendFlame retardant class V0, excellent light resistance, high impact resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature 0.000 °C |
10.3 ft-lb/in @Temperature 32.0 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND PSA 8500 V0 HF Flame Retardant PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendFlame retardant class V0, chlorine and bromine free, excellent light resistance, high impact resistance, excellent processabilityInformation pro.. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature 0.000 °C |
10.3 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTACARB 1060 V0 HF Flame Retardant Polycarbonate Flame retardant class V0, opaque, antimony, chlorine and bromine free, high impact resistance, high thermal resistance, good melt flow rate, good processability, good light resistanceInformation pro.. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature 23.0 °C |
10.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTACARB 1560 V0 Flame Retardant Polycarbonate Flame retardant class V0, antimony and PBDE free, opaque, high melt flow, high impact strength, high thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature 0.000 °C |
10.3 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTACARB 1560 V0 HF Flame Retardant Polycarbonate Flame retardant class V0, opaque, antimony, chlorine and bromine free, high impact resistance, high thermal resistance, good melt flow rate, good processability, good light resistanceInformation pro.. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature 23.0 °C |
10.3 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Carmel Olefins CAPILENE® SE 50 E Polypropylene Impact Copolymer Description: CAPILENE® SE 50 E is a low melt flow rate impact copolymer intended for sheet extrusion. It exhibits excellent impact strength even at low temperatures, combined with good processabi.. |
|||
Izod Impact, Notched | 5.49 J/cm @Thickness 3.20 mm |
10.3 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IMC-45 ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Izod Impact, Notched | 5.49 J/cm @Thickness 3.20 mm |
10.3 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IMC-45 ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |