Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SABIC PP 412MK49 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 412MK49 is specially developed for producing injection molded articles. This grade contains an antistatic & nucleating agents. It has medium flow properties, good impact r.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SABIC PP 413MNK45 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 413MNK45 is a controlled rheology PP grade with a very high fluidity. It is provided with an antistatic package & nucleating agent and is especially developed for producing.. |
|||
Izod Impact, Notched | 0.650 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
1.22 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PP 1370 PRE-ELEC PP 1370 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Asia Pacific) Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Europe-Africa-Middle East) Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTWM200 ASA ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® EFX830ME PC (Asia Pacific) Modified PC blend offering metallic look with minimal flow lines, flame retarded without using Chlorinated or Brominated additives.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -40.0 °C |
1.22 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LATAN 13 Medium Viscosity Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -40.0 °C |
1.22 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LASULF Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX8710 PPE+PA Noryl GTX8710 resin is a glass filled, high performance blend of PPE/PA that exhibits an exceptional balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-sta.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX8721 PPE+PA Noryl GTX GTX8721 resin is a glass and talc filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, conductivity, and low warpage. This .. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Asia Pacific) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Europe-Africa-Middle East) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-521 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -40.0 °C |
1.22 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-602G30 MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-777-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -40.0 °C |
1.22 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® TY-791HT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -40.0 °C |
1.22 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 1.7%); ASTM-D256 |
Toyobo GLAMIDE® NB-5550 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar GN077 Copolyester, Natural Eastar Copolyester GN077 is an amorphous resin with good melt strength, chemical resistance, high clarity and gloss. It is an excellent choice for extrusion blow molding small to intermediate size c.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -20.0 °C |
1.22 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Carmel Olefins CAPILENE® SG 50 Polypropylene Impact Copolymer Description: CAPILENE® SG 50 is a low melt flow rate impact copolymer suitable for injection molding applications. It exhibits good stiffness combined with high impact strength.Applications: CAP.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Carmel Olefins CAPILENE® HU 75 AV Polypropylene Impact Copolymer Description: CAPILENE® HU 75 AV is a nucleated and antistatic controlled rheology impact copolymer for injection molding. It is characterized by improved stiffness and medium impact resistance. .. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -40.0 °C |
1.22 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LARIL 13 G/30-V1 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |