Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.224 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.420 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Chi Mei Kibisan® PN137H SAN Resin, General Purpose Information provided by Calsak Corporation |
|||
Izod Impact, Notched | 0.224 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.420 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Chi Mei Kibisan® PN-127H SAN Chemical Resistant |