Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.700 - 1.10 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
1.31 - 2.06 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene |
|||
Izod Impact, Notched | 0.900 - 1.10 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.69 - 2.06 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon PC GF 10 V0 Polycarbonate, 10% Glass Fiber Characteristics: self-extinguishing V0 at 1,6 mm, 10% glass fibre filled |