Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.99 J/cm @Temperature -30.0 °C |
16.8 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® EXRL0684 PC Copolymer 7 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |