Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.66 J/cm @Temperature 23.0 °C |
14.4 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Europe-Africa-Middle East) Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |