Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
13.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT EX3600-0002 UV Black Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |