Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.35 J/cm @Temperature 0.000 °C |
11.9 ft-lb/in @Temperature 32.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTPM309 ASA+PC (Europe-Africa-Middle East) XTPM309 is a modified HRA170 with improved processing stability.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 6.35 J/cm @Temperature 23.0 °C |
11.9 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY HR-5006A Heat Resistant PC/ABS Alloy, Unreinforced, Weather Resistant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | 6.35 J/cm @Temperature 23.0 °C |
11.9 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY HR-5007AX Heat Resistant PC/ABS Alloy, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | 6.35 J/cm @Temperature 23.0 °C |
11.9 ft-lb/in @Temperature 73.4 °F |
3.2 mm (0.125 in) notch |
Kraton® G1651 + PPE blend (20/80) Blending KRATON D and G polymers with PPE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [.. |