Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.40 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
10.1 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa MAC-751 HF PC/ABS Alloy Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical .. |
|||
Izod Impact, Notched | 5.40 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
10.1 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa MAC-751 PC/ABS Alloy Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical .. |