Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.81 J/cm @Temperature -40.0 °C |
9.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PC/TP-GP3 PC/Polyester Alloy High Impact, Superior Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
9.00 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/ABS 2110 BK Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
9.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT IM 6200 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
9.01 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers ABSPC 7030-HES ABS/PC Injection Molding Grade, High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
9.01 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers DIAMALOY GLY 7010 Sheet Extrusion Grade Diamaloy GLY 7010 resin is a high-gloss, high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, a.. |
|||
Izod Impact, Notched | 4.81 J/cm @Temperature -20.0 °C |
9.00 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Dow AFFINITY™ SM 1300G Polyolefin Plastomer (POP) AFFINITY™ SM 1300G is an ethylene alpha-olefin resin for Injection Molding is produced via INSITE™ Technology from Dow Plastics. The resin offers excellent performance in durable injection molded.. |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 6.35 mm, Temperature -17.8 °C |
9.00 ft-lb/in @Thickness 0.250 in, Temperature 0.000 °F |
ASTM D-256 |
Axiall 7801 Rigid PVC, Extrusion, White, High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 6.35 mm, Temperature -17.8 °C |
9.00 ft-lb/in @Thickness 0.250 in, Temperature 0.000 °F |
ASTM D-256 |
Axiall 7803 Rigid PVC, Extrusion High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |