Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.30 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
8.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L0189 Polyvinyl Chloride, Rigid (PVC, Rigid) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Izod Impact, Notched | 4.30 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
8.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5700 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Izod Impact, Notched | 4.30 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
8.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5730 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Izod Impact, Notched | 4.30 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
8.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5731 Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. Dark colored compounds do not.. |
|||
Izod Impact, Notched | 4.30 J/cm @Temperature -30.0 °C |
8.06 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 4.30 J/cm @Temperature -30.0 °C |
8.06 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Asia Pacific) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 4.30 J/cm @Temperature -30.0 °C |
8.06 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Europe-Africa-Middle East) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East re.. |
|||
Izod Impact, Notched | 4.30 J/cm @Temperature -30.0 °C |
8.06 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Europe-Africa-Middle East) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur.. |
|||
Izod Impact, Notched | 4.30 J/cm @Temperature 23.0 °C |
8.06 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 4009 Acrylonitrile Butadiene Styrene ABS with high impact resistanceHigh impact resistance at low temperature, high gloss, good processabilityInformation provided by Cossa Polimeri S.r.l. |