Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.66 J/cm @Thickness 6.35 mm |
6.86 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chi Mei Polylac® PA-747 ABS High impact |