Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.85 J/cm @Temperature 0.000 °C |
5.34 ft-lb/in @Temperature 32.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTPM302 ASA+PC (Europe-Africa-Middle East) XTPM302 is a general purpose ASA/PC injection moulding grade, available in various colors.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |