Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.46 J/cm @Temperature -30.0 °C |
4.61 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by .. |
|||
Izod Impact, Notched | 2.46 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
4.60 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF33 IM3 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 2.46 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
4.60 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES HiFill® PP CO GF30 CC 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.46 J/cm @Thickness 3.17 mm |
4.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.46 J/cm @Thickness 3.17 mm |
4.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.46 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
4.60 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES HiFill® PP CO GF20 CC 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.46 J/cm @Temperature 23.0 °C |
4.61 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Verton RV008ESV_GY7E072 PA 66 Preliminary data for 40% long glass fiber filled, single color pellet gray, PA66This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 2.46 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
4.60 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Chi Mei Kibilac® PW-978B ASA, High Heat Acrylonitrile/Styrene/AcrylateInformation provided by Calsak Corporation |
|||
Izod Impact, Notched | 2.46 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
4.61 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer Diamaloy GLY 7510 resin is a high gloss, high heat and high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. This product is rated f1 by UL and be customed.. |
|||
Izod Impact, Notched | 2.46 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
4.60 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Chi Mei Kibilac® PW-978D ASA, High Heat
(discontinued **) Acrylonitrile/Styrene/AcrylateInformation provided by Calsak Corporation |