Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.08 J/cm @Thickness 12.7 mm, Temperature 23.0 °C |
3.90 ft-lb/in @Thickness 0.500 in, Temperature 73.4 °F |
ASTM-D256 |
Ineos ABS Lustran® 433 ABS, General-Purpose Injection Molding Grade Lustran® ABS 433 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is a high-impact, high-gloss ABS, available only in natural (000000) and black (904000)... |
|||
Izod Impact, Notched | 2.08 J/cm @Temperature 23.0 °C |
3.90 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
MRC Polymers SATRANâ„¢ 805 ABS Terpolymer, Impact Modified Information provided by MRC Polymers Inc. |
|||
Izod Impact, Notched | 2.08 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.90 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF33 IM2 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 2.08 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.90 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF14 IM HS L 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Izod Impact, Notched | 2.08 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.90 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF14 IM L 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedUL File Nu.. |
|||
Izod Impact, Notched | 2.08 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.90 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES HiFill® PA6 LGF30 HS L 12mm 30% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedIn.. |
|||
Izod Impact, Notched | 2.08 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
3.90 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers Centrex® HGM Automotive Grade, Injection Molding Grade Centrex HGM resin is an exceptionally high-gloss grade of ASA (acrylonitrile-styrene-acrylate). This injection molding grade has excellent gloss retention, excellent resistance to chemicals and high.. |