Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HI121H ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HI153 ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm, Temperature -40.0 °C |
3.67 ft-lb/in @Thickness 0.252 in, Temperature -40.0 °F |
ASTM D256 |
LG Chemical KEYFLEX BT 1155D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LG703W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided.. |
|||
Izod Impact, Notched | >= 1.96 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 3.67 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL EI5002L PP Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 9002-88-4Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 1.96 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 3.67 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HI5204 PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 1.96 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
>= 3.67 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LUPOY HI1002ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical AF308 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.17 mm |
3.67 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® CA-7009 PA/PPE, Antistatic Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
3.67 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.17 mm |
3.67 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced Anti-staticInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm |
3.67 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® GC-0770 H ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm |
3.67 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® LX-0971 S ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.17 mm |
3.67 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VS-0800 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
3.67 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
3.67 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm |
3.67 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced Anti-staticInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.17 mm |
3.67 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced Anti-staticInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm |
3.67 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® LX-0935 S ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Temperature -20.0 °C |
3.67 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H1000PWI High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weathering, reduce heat conductivity to waterRecommended Applications: Above ground pipes, double wall pipesInforma.. |
|||
Izod Impact, Notched | 1.96 J/cm @Temperature -20.0 °C |
3.67 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H1000PYL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE100 pipe, non pressure pipesCertification: Certified by LNE.. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 100V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 240V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 240Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 500Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm |
3.67 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM-16M ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm |
3.67 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron SE-22 FR Flame Retardant ABS Grade Information provided by Bhansali |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm |
3.67 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron AN-312 Flame Retardant ABS Grade |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm |
3.67 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron KU602 ABS Heat Resistant High ImpactInformation provided by Bhansali |