Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.80 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
3.37 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LI-943 ASA Resin
(discontinued **) Heat resistance, Excellent weather resistance, Well balanced mechanical properties, Superior chemical resistance, Good thermal aging stability, Good moldability and processability, Applications incl.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature 23.0 °C |
3.37 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon DX07323 PC+ABS LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp ML4351HF PC (Asia Pacific) LNP* Thermocomp* ML4351HF is a Light Reflecting Grade.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -18.0 °C |
3.37 ft-lb/in @Temperature -0.400 °F |
ASTM Test |
Styrolution Terluran® HI-10 ABS Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature 23.0 °C |
3.37 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 1.25%); ASTM-D256 |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -40.0 °C |
3.37 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 2.9%); ASTM-D256 |
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature 23.0 °C |
3.37 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 1.0%); ASTM-D256 |
Toyobo GLAMIDE® TY-791GT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature 23.0 °C |
3.37 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 0.8%); ASTM-D256 |
Toyobo GLAMIDE® TY-592GHV 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature 23.0 °C |
3.37 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 0425 GFS Acrylonitrile Butadiene Styrene, 13% Glass Filled ABS with 13% short glass fiberExcellent mechanical and thermal propertiesInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature 0.000 °C |
3.37 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 1030 V0/Ex Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high impact resistance, high gloss, good light resistance, for extrusionInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.80 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
3.37 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epiryl B PPO Polyphenylene oxide |
|||
Izod Impact, Notched | 1.80 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
3.37 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epiryl PPO V0 Polyphenylene oxide Characteristics: self-extinguishing V0 at 1,6 mm |