Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical KEYFLEX BT 1172D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 2.76 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HI5302R PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
2.76 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical Lupox® TE5000H PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
2.76 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical Lupox® TE5000HU PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 26062-94-2, 137050-02-03 and 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
2.76 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical Lupox® TE5000S PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Roof Rack)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Information provided.. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm |
2.75 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
LG Chemical SI-610 Alphalac Polystyrene High flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include big size electric app.. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
2.76 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1098 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® BF-0370 MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in the exterior of electric products and household appliancesInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® LH-0300 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm |
2.76 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HF-3200H PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm |
2.76 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® LX-0957 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® LH-1070W PC, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 200H Modified Polyphenylene Ether Heat ResistantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 220Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 240Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 500V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 500Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.20 mm |
2.76 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron AN480V2 Flame Retardant ABS Grade Information provided by Bhansali |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm |
2.76 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM17V ABS Injection Molding Grade Super High Gloss, Medium ImpactInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 600H Modified Polyphenylene Ether Heat ResistantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm |
2.76 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-17A(DLW) ABS Injection Molding Grade Medium Impact, Medium Flow ,White UndertoneInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm |
2.76 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-17A(HF) ABS Injection Molding Grade Very High Flow, Medium Impact GradeInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm |
2.76 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM21V ABS Injection Molding Grade Super High Gloss, High RigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm |
2.76 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron SHF-50+M ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.20 mm |
2.76 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron KU602M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
2.76 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® TK-2046HM PCT, 40% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm |
2.76 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-17A(DLW) ABS Injection Molding Grade Medium Impact, Medium Flow ,White UndertoneInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.20 mm |
2.76 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IPM3000 PMMA- ABS Alloy Super High Gloss, High scratch resistanceInformation provided by Bhansali |