Izod Impact, Notched 1.295 J/cm

@Temperature 0.000 °C
2.426 ft-lb/in

@Temperature 32.0 °F
JIS-K-6740
Denka VINYKON R4105 PVC, R grade for hard extrusion
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Izod Impact, Notched 1.295 J/cm

@Temperature 23.0 °C
2.426 ft-lb/in

@Temperature 73.4 °F
JIS-K-6740
Denka VINYKON R3102 PVC, R grade for hard extrusion
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..