Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.00 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.87 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ISO 180/4A |
Polimeri Europa Sinkral® B 432/E ABS Resin Sinkral B 432/E is a general purpose extrusion grade which exhibits a good balance between rigidity and toughness. Designation: Thermoplastic ISO 2580-ABS 1,EGN,105-04-16-20Applications: Large sheet.. |
|||
Izod Impact, Notched | 1.00 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.87 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ISO 180/4A |
Polimeri Europa Sinkral® C 442 ABS Resin Sinkral C 442 is a heat resistant injection molding grade offering good flow and impact resistance together with excellent thermal stability during processing. Designation: Thermoplastic ISO 2580-AB.. |
|||
Izod Impact, Notched | 1.00 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
1.87 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ISO 180/4A |
Polimeri Europa Sinkral® PD L 322 ABS Resin Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.Applications: Widely used in the small and.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® EFX810ME PC Modified PC blend offering metallic / sparkle look with minimal flowline visibility.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering high modulus / low CTE and good practical impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle .. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Izod Impact, Notched | 1.00 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
1.87 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ASTM D256 |
Mapal Plastics Maplon Type S Polypropylene Sheet Properties: Low stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printingApplications: Stationery, Packaging, House-hold productsand printed items |
|||
Izod Impact, Notched | >= 1.00 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
>= 1.87 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Kingfa LONOY 1600 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Izod Impact, Notched | 1.00 J/cm @Thickness 3.17 mm, Temperature -29.0 °C |
1.87 ft-lb/in @Thickness 0.125 in, Temperature -20.2 °F |
notch |
Kraton® FG1901 + PBT blend (30/70), UV aged Carbon arc weatherometer UV aging for 360 hours. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A-B]n). The KRATON G series are second generation block polymers .. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -40.0 °C |
1.87 ft-lb/in @Temperature -40.0 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon DX07323 PC+ABS LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -18.0 °C |
1.87 ft-lb/in @Temperature -0.400 °F |
ASTM Test |
Styrolution Terluran® GP-22 ABS Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -40.0 °C |
1.87 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-656E Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND 0840 GF Polycarbonate ABS Blend, 20% Glass Filled Polycarbonate and Acrylonitrile Butadiene Styrene blend with 20% glass fiber reinforcementHigh dimensional stability, high stiffnessInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -40.0 °C |
1.87 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 383A2R30010 Cellulose Acetate Propionate, Natural, Trsp Applications:Oral HygienePlastics for hygiene feminine productsRecreationalToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 0.000 °C |
1.87 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTACARB 0820 GF V0-5V HF Flame Retardant Polycarbonate Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, antimony, chlorine and bromine free, high stiffness, high dimensional stability, good melt flow rate, good processability, g.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 0.000 °C |
1.87 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 0615 HHT Acrylonitrile Butadiene Styrene ABS with very high heat resistanceGood impact resistance, stiff, excellent surface appearance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 0.000 °C |
1.87 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 0815 HHT Acrylonitrile Butadiene Styrene ABS with very high heat resistanceGood melt flow rate, good impact resistance, excellent surface appearance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP H 0540 GFC Polypropylene, 20% Glass Filled PP homopolymer 20% chemically coupled glass fiber reinforcedInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -20.0 °C |
1.87 ft-lb/in @Temperature -4.00 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 0580 GFC Polypropylene, 40% Glass Filled PP homopolymer 40% chemically coupled glass fiberExcellent stiffness, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP H 1660 GFC Polypropylene, 30% Glass Filled PP homopolymer 30% chemically coupled glass fiber reinforcedHigh melt flow rate, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.00 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.87 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epicarb PC BLACK IQ Polycarbonate Characteristics: good fluidity, good impact, industrial quality |
|||
Izod Impact, Notched | 1.00 - 1.80 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.87 - 3.37 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon FR-PC V0 Polycarbonate Characteristics: self-extinguishing V0 at 1,6 mm |
|||
Izod Impact, Notched | 1.00 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.87 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon G2-PC 10% GF Polycarbonate, 10% Glass Fiber Characteristics: 10% glass fibre filled, good mechanical properties |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -20.0 °C |
1.87 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Carmel Olefins CAPILENE® TR 50 Polypropylene Impact Copolymer Description: CAPILENE® TR 50 is a medium melt flow rate heterophasic copolymer with very high impact strength, even at low temperature, designed for injection molding. This grade combines good pr.. |