Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.853 J/cm @Thickness 3.17 mm |
1.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GP-5300G PBT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.853 J/cm @Thickness 6.35 mm |
1.60 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled Material with 10% GF reinforcement with high stiffness that can be used in refrigerator vegetable boxesInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.853 J/cm @Thickness 3.17 mm |
1.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GP-5300G PBT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.853 J/cm @Thickness 6.35 mm |
1.60 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled Material with 10% GF reinforcement with high stiffness that can be used in refrigerator vegetable boxesInformation provided by Samsung Cheil Industries. |