Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.750 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87560 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.41 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ISO 180/4A |
Polimeri Europa Sinkral® PD D 232/M4 ABS Resin Special very low gloss extrusion / co-extrusion grade, with good flow.Applications: Sinkral PD D 232/M4 is widely used in extrusion / co-extrusion of foils, when a very high matte appearance is req.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PBT 1455 PRE-ELEC PBT 1455 is a conductive thermoplastic compound based on PBT. Conductivity is achieved by using special conductive carbon black. PRE-ELEC PBT 1455 has excellent mechanical properties as wel.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -30.0 °C |
1.41 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY5105 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTWE280 ASA Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTWE280 ASA (Europe-Africa-Middle East) Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -40.0 °C |
1.41 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar 5445 PCTG Copolyester, Injection Molded
(discontinued **) Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -20.0 °C |
1.41 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTWE280 ASA (Asia Pacific) Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PPE 1461
(discontinued **) PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.41 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ISO 180/4A |
Polimeri Europa Sinkral® D 232/M3 ABS Resin
(discontinued **) Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extr.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -20.0 °C |
1.41 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
LATI LASULF Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LASULF Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
50%RH; ASTM D256 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® TY-791HT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -40.0 °C |
1.41 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 307E0V16310 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
1.41 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Diamond Polymers Centrex® 814 General Purpose Injection Molding Grade Centrex 814 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and processing perfor.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Carmel Olefins CAPILENE® SW 75 AV Polypropylene Impact Copolymer Description: CAPILENE® SW 75 AV is a high melt flow rate, controlled rheology impact copolymer for injection molding. CAPILENE® SW 75 AV is nucleated with antistatic additivation. It is characte.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LASTIROL TR G/10-V1 10% Glass Fiber Reinforced Polystyrene (PS) (UL94 V-1)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -40.0 °C |
1.41 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LASULF G/20 20% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -40.0 °C |
1.41 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LARTON G/30 30% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -20.0 °C |
1.41 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
LATI LARTON G/30 30% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARTON G/30 30% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |