Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.640 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.20 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87345 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.640 J/cm @Thickness 3.18 mm, Temperature -40.0 °C |
1.20 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L0676 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Izod Impact, Notched | 0.640 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.20 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Fittings M1012 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature -40.0 °C |
1.20 ft-lb/in @Temperature -40.0 °F |
|
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature 77.0 °C |
1.20 ft-lb/in @Temperature 171 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.640 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.20 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM-D256 |
Ineos ABS Lustran® 433 ABS, General-Purpose Injection Molding Grade Lustran® ABS 433 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is a high-impact, high-gloss ABS, available only in natural (000000) and black (904000)... |
|||
Izod Impact, Notched | 0.640 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.20 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM-D256 |
Ineos ABS Lustran® 633 ABS, Injection Molding Grade Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical .. |
|||
Izod Impact, Notched | 0.640 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LG Chemical MI-750 MIPS Medium impact |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature -30.0 °C |
1.20 ft-lb/in @Temperature -22.0 °F |
3.2 mm (0.125 in) notch |
Kraton® G1652 + PP blend + Talc (12/21/67) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Izod Impact, Notched | 0.640 J/cm @Thickness 6.35 mm |
1.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
LG Chemical 401 AF Flame Retardant HIPS NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, uses non-bromide as fl.. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature 23.0 °C |
1.20 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 2210K PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature -30.0 °C |
1.20 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 2210K PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature 23.0 °C |
1.20 ft-lb/in @Temperature 73.4 °F |
Compression Molded; ASTM D256 |
Styron STYRONâ„¢ 6500 Ignition Resistant Polystyrene Resin Overview: STYRONâ„¢ 6500 is an ignition-resistant polystyrene resin with excellent balance of strength, heat resistance and flow properties that are tailor-made for consumer electronics applicati.. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature -30.0 °C |
1.20 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature -30.0 °C |
1.20 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Asia Pacific) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature -30.0 °C |
1.20 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature 23.0 °C |
1.20 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-400G15 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature -40.0 °C |
1.20 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy Type: Estaloc® 61225 Alloy RETPU is a polyester-type thermoplastic alloy.Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.Uses: Injection molding.Availa.. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature -40.0 °C |
1.20 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar MN004 Copolyester Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl.. |
|||
Izod Impact, Notched | 0.640 J/cm @Thickness 3.17 mm, Temperature -18.0 °C |
1.20 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
ASTM D256 |
Diamond Polymers Centrex® 485 Sheet Extrusion Grade Centrex 485 resin is a low-gloss, medium-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it.. |