Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.630 J/cm @Temperature -40.0 °C |
1.18 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Aspira EB062 Copolyester Resin for Extrusion Blown Bottles Applications:Beverage packagingBottlesExtrusion blow moldingFood packagingPersonal care bottlesKey Attributes:Easy to extrude, cut, print and sealEffective barrier propertiesExcellent chemical resis.. |
|||
Izod Impact, Notched | 0.630 J/cm @Temperature -40.0 °C |
1.18 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar EB062 Copolyester Eastar Copolyester EB062 is a resin specifically developed for extrusion blown bottles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to com.. |
|||
Izod Impact, Notched | 0.630 J/cm @Temperature -40.0 °C |
1.18 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar MB002 Copolyester Eastar copolyester MB002 is a resin specifically developed for extrusion blow molding containers in medical applications where aesthetics such as high clarity and gloss, coupled with high toughness .. |
|||
Izod Impact, Notched | 0.630 J/cm @Temperature -40.0 °C |
1.18 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Provista MP002 Copolymer Provista Copolymer MP002 is a resin specifically developed for extrusion into profiles for medical applications where aesthetics such as high clarity and gloss, coupled with design flexibility and e.. |
|||
Izod Impact, Notched | 0.630 J/cm @Temperature -40.0 °C |
1.18 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Provista ST Copolymer Provista Copolymer ST is a resin specifically developed for profile extrusion where high clarity and gloss, toughness, and processability are critical. Provista Copolymer ST is a second-generation m.. |
|||
Izod Impact, Notched | 0.630 J/cm @Temperature -40.0 °C |
1.18 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar GN078 Copolyester, Natural Eastar Copolyester GN078 builds on the strength of Eastar Copolyester GN077 by offering improved melt strength and toughness. Eastar Copolyester GN078 does not meet FDA compliance but is an excellen.. |
|||
Izod Impact, Notched | 0.630 J/cm @Temperature 23.0 °C |
1.18 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem CP 191 Injection Molding Polypropylene Applications: Household; low temperature packing; frozen desserts packaging. Information provided by Braskem |