Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.420 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
0.787 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PS 1326 PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature -30.0 °C |
0.787 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTWE280 ASA Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature -30.0 °C |
0.787 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTWE280 ASA (Europe-Africa-Middle East) Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX9254 PC Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Asia Pacific) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Europe-Africa-Middle East) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature -30.0 °C |
0.787 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTWE280 ASA (Asia Pacific) Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Asia Pacific region. |