Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.270 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
0.506 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5100 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Izod Impact, Notched | 0.270 J/cm @Temperature -30.0 °C |
0.506 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTWE480 ASA (Asia Pacific) Anti-scratch Geloy grade with excellent weatherability, high flow, and good surface quality. XTWE480 is available in various colours.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.270 J/cm @Temperature -40.0 °C |
0.506 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar GN125 Copolyester, Natural
(discontinued **) Eastar Copolyester GN125 is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet light inhibitor. This product is recommended for indoor applications requiring enhanced co.. |
|||
Izod Impact, Notched | 0.270 J/cm @Temperature -40.0 °C |
0.506 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Izod Impact, Notched | 0.270 J/cm @Temperature -40.0 °C |
0.506 ft-lb/in @Temperature -40.0 °F |
50%RH; ASTM D256 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.270 J/cm @Temperature -40.0 °C |
0.506 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar EN001 Copolyester Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro.. |
|||
Izod Impact, Notched | 0.270 J/cm @Temperature -40.0 °C |
0.506 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar MN021 Copolyester Eastar copolyester MN021 is a thermoplastic condensation copolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Izod Impact, Notched | 0.270 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
0.506 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Diamond Polymers Centrex® 821 ASA Weatherable Polymers Injection Molding Grade Centrex 821 resin is a medium-gloss, high-heat, medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and pr.. |
|||
Izod Impact, Notched | 0.270 J/cm @Temperature -40.0 °C |
0.506 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con.. |
|||
Izod Impact, Notched | 0.270 J/cm @Temperature -40.0 °C |
0.506 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman 9921W PET Injection Molded
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |