Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.250 J/cm @Temperature -30.0 °C |
0.468 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX9254 PC Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature -30.0 °C |
0.468 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Asia Pacific) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature -30.0 °C |
0.468 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Europe-Africa-Middle East) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Izod Impact, Notched | 0.250 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.468 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Izod Impact, Notched | 0.250 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.468 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Solvay Specialty Polymers Halar® 1400LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: FibersAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 300 °CInformation provided by Solvay Spec.. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature 0.000 °C |
0.468 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP 1000 V2 H Flame Retardant Polypropylene PP homopolymerFlame retardant class V2, PBDE free, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature 0.000 °C |
0.468 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP 1040 V2 K Flame Retardant Polypropylene PP copolymerFlame retardant class V2, halogen free, good mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature 23.0 °C |
0.468 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP 1050 V0 HF H Flame Retardant Polypropylene PP homopolymerFlame retardant class V0, halogen free, excellent mechanical characteristics, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature 0.000 °C |
0.468 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 0360 T8 Polypropylene, 30% Mineral Filled PP homopolymer 30% mineral fillerExtrusion gradeInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature 0.000 °C |
0.468 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 10100 BS Polypropylene, 50% Mineral Filled PP homopolymer 50% mineral fillerExcellent surface appearance, high densityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature 0.000 °C |
0.468 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 1080 T6 T D Polypropylene, 40% Mineral Filled PP homopolymer 40% mineral fillerGood physical and mechanical characteristics, high thermal stability, detergent resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature 0.000 °C |
0.468 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 2550 CBS/E Polypropylene, 25% Mineral Filled PP homopolymer 25% mineral fillerHigh gloss, very high melt flow rate, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature 0.000 °C |
0.468 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 2560 C Polypropylene, 30% Mineral Filled PP homopolymer 30% mineral fillerExcellent processability, good surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature 0.000 °C |
0.468 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP HK 2540 T8 Polypropylene, 20% Mineral Filled PP homo/copolymer 20% mineral fillerGood physical and mechanical propertiesInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature -20.0 °C |
0.468 ft-lb/in @Temperature -4.00 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP K 0200 V2 Flame Retardant Polypropylene PP copolymer extrusion gradeFlame retardant class V2, PBDE free, good impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature -20.0 °C |
0.468 ft-lb/in @Temperature -4.00 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP K 1280 T8 Polypropylene, 40% Mineral Filled PP copolymer 40% mineral fillerExcellent physical and mechanical characteristics, good surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature 0.000 °C |
0.468 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTASAN SAN 0840 GF Styrene Acrylonitrile SAN with 20% glass fiber reinforcementExcellent dimensional stability, good heat resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature -20.0 °C |
0.468 ft-lb/in @Temperature -4.00 °F |
ASTM D256A |
Braskem CP 401 HC Injection Molding Polypropylene Description: CP 401HC is a medium melt flow rate heterophasic copolymer, specially designed to achieve high stiffness/impact strength balance. This product offers good surface appearance and process.. |