Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSD11 Normal Grade Heat Sealable Film (thickness: 18 µm) HSD11 is a general, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dim.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSD12 Normal Grade Heat Sealable Film (thickness: 18 µm) HSD12 is a printing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona trea.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSD12 Normal Grade Heat Sealable Film (thickness: 25 µm) HSD12 is a printing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona trea.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSD12 Normal Grade Heat Sealable Film (thickness: 30 µm) HSD12 is a printing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona trea.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 18 µm) HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 20 µm) HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 25 µm) HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 30 µm) HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSS11 Normal Grade Heat Sealable Film (thickness: 18 µm) HSS11 is a general, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dimens.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSS11 Normal Grade Heat Sealable Film (thickness: 20 µm) HSS11 is a general, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dimens.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSS11 Normal Grade Heat Sealable Film (thickness: 25 µm) HSS11 is a general, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dimens.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSS11 Normal Grade Heat Sealable Film (thickness: 30 µm) HSS11 is a general, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dimens.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSS12 Normal Grade Heat Sealable Film (thickness: 20 µm) HSS12 is a printing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona treatme.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSS12 Normal Grade Heat Sealable Film (thickness: 30 µm) HSS12 is a printing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona treatme.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSS13 Normal Grade Heat Sealable Film (thickness: 18 µm) HSS13 is a metalizing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSS13 Normal Grade Heat Sealable Film (thickness: 20 µm) HSS13 is a metalizing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead HSS13 Normal Grade Heat Sealable Film (thickness: 30 µm) HSS13 is a metalizing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength | 517.9 g/25 mm | 1.142 lb/in | Kinlead |
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side .. |