Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hot Tack Strength | 1800 - 3000 g/25 mm | 1800 - 3000 g/in | Average value: 2200 g/25 mm Grade Count:21 |
Overview of materials for Ionomer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |