Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hot Tack Strength | 1400 g/25 mm | 1400 g/in | seal bar 115°C; Packforsk method. |
DuPont Nucrel® 403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 4 wt% Methacrylic Acid.Nucrel® 0403 is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene res.. |
|||
Hot Tack Strength | 1400 - 1800 g/25 mm | 1400 - 1800 g/in | Average value: 1720 g/25 mm Grade Count:5 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Film Grade". Each property range of values reported is minimum and m.. |