| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| SABIC Innovative Plastics Cycoloy® CE1821 PC+ABS (Europe-Africa-Middle East) High stiffness PC/ABS blend offering high impact, high heat, low CTE, good surface quality and excellent extrusion and thermoforming characteristics.This data was supplied by SABIC-IP for the Europe.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Asia Pacific) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| SABIC Innovative Plastics Lexan® AD4820 PC LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin.This data was supplied by SABIC-IP for the America.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| SABIC Innovative Plastics Lexan® IFX2420Z PC (Asia Pacific) Lexan* IFX2420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware applications specifically for welding. This grades .. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| SABIC Innovative Plastics Lexan® IFX6420Z PC (Asia Pacific) Lexan* IFX6420Z is a medium viscosity, release containing, injection moldable, polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grades meets the transm.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
| SABIC Innovative Plastics PC0700 PC PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
| SABIC Innovative Plastics PC0700 PC (Europe-Africa-Middle East) PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
| SABIC Innovative Plastics PC0703 PC PC0703 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product designed for use in the extrusion market.This data was supplied by SABIC-IP for the Americas reg.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
| SABIC Innovative Plastics PC0800 PC PC0800 resin is a low flow (MFR = 8 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
| SABIC Innovative Plastics PC1000 PC PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
| SABIC Innovative Plastics PC1000 PC (Asia Pacific) PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
| SABIC Innovative Plastics PC1000R PC PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
| SABIC Innovative Plastics PC1000R PC (Asia Pacific) PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
| SABIC Innovative Plastics PC1003R PC PC1003R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was .. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
| SABIC Innovative Plastics PC1500 PC PC1500 resin is a medium-high flow (MFR = 15 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold .. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
| SABIC Innovative Plastics PC1800 PC PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold .. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
| SABIC Innovative Plastics PC1800 PC (Asia Pacific) PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold .. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
| SABIC Innovative Plastics PC1800 PC (Europe-Africa-Middle East) PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold .. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
| SABIC Innovative Plastics PC1800R PC PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli.. |
|||
| Impact Test | 65.0 J | 47.9 ft-lb | Multiaxial Impact; ISO 6603 |
| SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66 LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact, Wear Resistant. |
|||
| Impact Test | 65.0 J | 47.9 ft-lb | Multiaxial Impact; ISO 6603 |
| SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
| Impact Test | 65.0 J | 47.9 ft-lb | Multiaxial Impact; ISO 6603 |
| SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
| Impact Test | 65.0 J | 47.9 ft-lb | Multiaxial Impact; ISO 6603 |
| SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Asia Pacific) LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
| Impact Test | 65.0 J @Thickness 3.20 mm |
47.9 ft-lb @Thickness 0.126 in |
Instrumented total energy; 3.2 mm thick; 0.5 in. dart; 3 in. clamp; 15 mph; ASTM D3763 |
| Covestro Makrolon® DP 1-1456 Polycarbonate, Impact Grade Impact modified injection molding grade, extremely easy flow and easy mold release, for thin walled applications with long flow lengths.Information provided by Bayer.As of 1 September 2015, Bayer Ma.. |
|||
| Impact Test | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| SABIC Innovative Plastics Xenoy® X6320 PBT+PC X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.This data was supplied by SABIC-IP.. |
|||