Impact Test 11.3 - 22.6 J
8.33 - 16.7 ft-lb
Torque Break
Ritelok TL42 Nutlock
Anaerobic. Medium strength threadlocker for screws, nuts and bolts. Prevent corrosion, Vibration resistant, Dismantle using normal tools
Impact Test 16.9 - 22.6 J
12.5 - 16.7 ft-lb
Torque Break
Ritelok TL62 Studlock
Anaerobic. High Strength studlock for heavy duty items, vibration & stress load. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant
Impact Test 11.3 - 22.6 J
8.33 - 16.7 ft-lb
Break
ND Industries NutGrade® 121 Removable Threadlocker
A medium strength threadlocker. Seals most types of nuts and bolts allowing disassembly using standard tools.Typical Usesstuds and bolts, threaded pipe fittings, and locking nuts or bolts larger th..
Impact Test 11.3 - 22.6 J
8.33 - 16.7 ft-lb
Torque Break
Ritelok TL41 Oil Tolerant Threadlocker
Anaerobic. Medium strength threadlocker. Designed to lock oily fasteners. Prevent corrosion, Vibration resistant, Dismantle using normal tools