Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 7.10 J | 5.24 ft-lb | TUP Impact; 1" radius tip on 1/16" plaque |
Ineos H28E-00 Polypropylene Homopolymer, Antistatic Grade H28E-00 is an antistated, controlled rheology polypropylene homopolymer. It is designed for injection molding applications that require improved impact. This material meets the Food and Drug.. |