Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 63.0 J @Temperature 23.0 °C |
46.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
Impact Test | 63.0 J @Temperature 23.0 °C |
46.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Cycoloy® CY2000 PC+ABS Cycoloy resin CY2000 is a flame retardant (FR) PC/ABS blend free from halogen containing FR agents. It was designed to meet CA133 application requirements.This data was supplied by SABIC-IP for the .. |
|||
Impact Test | 63.0 J @Temperature 23.0 °C |
46.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® FXD104R PC (Europe-Africa-Middle East) FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Impact Test | 63.0 J @Temperature 23.0 °C |
46.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Lexan® I2220 PC General purpose polycarbonate with melt flow rate of 10.5.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 63.0 J @Temperature 23.0 °C |
46.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® IR2240 PC UL rated HB. 200 series recommended when V-2 rating required. Nonhalogenated. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for.. |
|||
Impact Test | 63.0 J @Temperature 23.0 °C |
46.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Lexan® IR2520 PC General purpose polycarbonate with melt flow rate of 8.5.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 63.0 J @Temperature 23.0 °C |
46.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Lexan® OQ2320 PC Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent quality production control.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 63.0 J @Temperature 23.0 °C |
46.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Lexan® OQ2320 PC (Asia Pacific) Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent quality production control.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 63.0 J @Temperature 23.0 °C |
46.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Lexan® VR2520 PC General purpose polycarbonate with melt flow rate of 8.5.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 63.0 J @Temperature 23.0 °C |
46.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Lexan® 141S PC (Asia Pacific) Nonhalogenated. 10.5 MFR. Internal mold release.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 63.0 J @Temperature 23.0 °C |
46.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Europe-Africa-Middle East) Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors.This data was supplied b.. |
|||
Impact Test | 63.0 J @Temperature 23.0 °C |
46.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific) Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di.. |
|||
Impact Test | 63.0 J | 46.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE LNP* STAT-KON* FX98500 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Impact Test | 63.0 J | 46.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific) LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Impact Test | 63.0 J | 46.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON DX02437 PC (Asia Pacific) LNP Stat-Kon DX02437 is a compound based on Polycarbonate resin containing conductive carbon powder, with good impact-resistance, flow and ESD performance, suitable for semi-con industry. |
|||
Impact Test | 63.0 J | 46.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific) LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Impact Test | 63.0 J | 46.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE LNP* STAT-KON* FX98500C is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |