Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing 30% Mixed Glass, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36EU PC LNP* Lubricomp* DFL36EU is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Easy Molding and UV Stabilized. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU (Asia Pacific) LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Impact Test | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp PL004 PA 6 LNP* Lubricomp* PL004 is a compound based on Nylon 6 containing PTFE Lubricant. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 (Asia Pacific) LNP* Lubricomp* RFP36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. This product is also known as Lub.. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON DD0009E PC LNP* STAT-KON* DD0009E is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant, Easy Molding. |
|||
Impact Test | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp AF0029 ABS LNP* Thermocomp* AF0029 is an ABS base resin containing Glass Fiber. Characteristics of this grade are Flame Retardancy.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP DF0049E PC (Asia Pacific) LNP* Thermocomp* DF0049E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Easy Molding, Flame Retardant. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Thermocomp MX88073 PP (Asia Pacific) LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp RF0059 PA 66 (Asia Pacific) LNP STARFLAM* RF0059 is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP for t.. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR (Asia Pacific) LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP UC008H PPA LNP THERMOCOMP* UC008H is a compound based on Polyphthalamide resin containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Thermocomp UC008S PPA (Asia Pacific) LNP* Thermocomp* UC008S is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for.. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOTUF IX02582 PA6.12 LNP* Thermotuf* IX02582 is a compound based on Nylon 6/12 resin containing Proprietary Filler(s). Added features of this material include: High Impact. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOTUF RF006I PA 66 LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Impact Test | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Asia Pacific) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Impact Test | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Europe-Africa-Middle East) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Impact Test | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp KFI12A Acetal Homopolymer LNP LUBRICOMP* KFI12A is a compound based on Acetal Homopolymer resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABI.. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON DX05305C PC LNP* STAT-KON* DX05305C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP MC002 PP LNP* THERMOCOMP* MC002 is a compound based on Polypropylene resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Thermocomp MX88073 PP LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS (Asia Pacific) LNP* Thermocomp* NF004 is a compound based on PC+ABS Blend resin containing Glass Fiber. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOTUF VF008 Super Tough Nylon LNP THERMOTUF* VF008 is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP VERTON MVL36SX0 PP (Europe-Africa-Middle East) LNP* VERTON* MVL36SX0 is a compound based on PP resin containing Long Glass Fiber and PTFE. Added features include: Chemically coupled, Heat Stabilized, Internally Lubricated. |
|||
Impact Test | 5.00 J @Temperature -10.0 °C |
3.69 ft-lb @Temperature 14.0 °F |
Total Penetration Energy; ISO 6603-2 |
Borealis Borpact™ SE920MO Polypropylene Homopolymer for Injection Molding Borpact SE920MO is a high impact and transparent polypropylene. Borpact SE920MO is a new generation polypropylene having properties that were earlier not possible to combine. Borpact SE920MO offers.. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific) LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas re.. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON MFD03 PP (Asia Pacific) LNP* Stat-kon* MFD03 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Thermocomp UC008S PPA LNP* Thermocomp* UC008S is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for.. |