Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 244 J @Thickness 6.35 mm |
180 ft-lb @Thickness 0.250 in |
ARM |
ExxonMobil HDPE HD 8660.29 High Density Polyethylene Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Impact Test | 244 J @Thickness 6.35 mm |
180 ft-lb @Thickness 0.250 in |
ARM |
ExxonMobil HDPE HD P8660.29 High Density Polyethylene Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Impact Test | 244 J @Thickness 6.35 mm, Temperature -40.0 °C |
180 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
Impact Strength; Max Force; ARM |
ExxonMobil Escorene® LL-8302 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8302 is the base re.. |
|||
Impact Test | 244 J @Thickness 6.35 mm, Temperature -40.0 °C |
180 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
Impact Strength; Max Force; ARM |
ExxonMobil Escorene® LL-8361 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8361 is fully formu.. |