Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 78.0 J @Temperature 23.0 °C |
57.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® RL7517 PC FDA compliant (color limited). 2.5 MFR. Potable water/extrusion blowmolding applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 78.0 J @Temperature 23.0 °C |
57.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® EXRL0684 PC Copolymer 7 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |