Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP DFL32 PC LNP LUBRICOMP* DFL32 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Impact Test | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Geloy FXTW30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP FL003 PE LNP* LUBRICOMP* FL003 is a compound based on Polyethylene resin containing 15% PTFE. Added features include: Internally Lubricated. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP IFL36 PA6.12 LNP LUBRICOMP* IFL36 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Impact Test | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp KZL34 POM LNP* Lubricomp* KZL34 is a compound based on Acetal resin containing Milled Glass and PTFE. Characteristic of this grade is Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
Impact Test | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp OFB32I PPS LNP LUBRICOMP* OFB32I is a compound based on Polyphenylene Sulfide resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SA.. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 (Asia Pacific) LNP* Lubricomp* RFL34 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Impact Test | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp RP0049 PA 66 LNP LUBRICOMP* RP0049 is a compound based on Nylon 66 resin containing Flame Retardant, PTFE, Silicone. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP f.. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA12 LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON DE002ER PC LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON DE002ER PC (Asia Pacific) LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Stat-kon DE002P PC LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC (Asia Pacific) LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features of this material include: Clean Compounding System. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS LNP* STAT-LOY* A30009 is a compound based on ABS. Added features of this material include: Antistatic, Flame Retardant. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP DF006ER PC LNP THERMOCOMP* DF006ER is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES LNP THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing 20% Glass Fiber. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES (Asia Pacific) LNP* THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing Glass Fiber. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP JF004EXP PES LNP* THERMOCOMP* JF004EXP is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Impact Test | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp QF002 PA6.10 LNP* Thermocomp* QF002 is a compound based on Nylon 6/10 containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 (Asia Pacific) LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing Glass Bead. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP RX12402 PA 66 LNP* Thermocomp* RX12402 is a compound based on PA66 containing 60% Glass Fiber. Added feature is Superior Flow. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP VERTON MV005SX0 PP (Europe-Africa-Middle East) LNP* VERTON* MV005SX0 is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON REF42I PA 66 LNP* STAT-KON* REF42I is a compound based on Nylon 6/6 containing Proprietary Fillers. Added feature of this grade is: Electrically Conductive. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP RX98372H PA 66 LNP* Thermocomp* RX98372H is a compound based on Nylon 66 resin containing Proprietary Fillers. Characteristics of this grade are: Healthcare. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Thermocomp SF006S PA 12 LNP* Thermocomp* SF006S is a compound based on Nylon 12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
Impact Test | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp WB008 PBT LNP* Thermocomp* WB008 is a compound based on Thermoplastic Polyester (PBT) containing Glass Beads.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28EG PC LNP* Lubricomp* DFL28EG is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated, Easy Molding. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOTUF PF006I PA 6 LNP THERMOTUF* PF006I is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP JF004E PES LNP* THERMOCOMP* JF004E is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. |