Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 31.0 J @Thickness 2.50 mm |
22.9 ft-lb @Thickness 0.0984 in |
Instrumented Impact, Total Energy; 2.5 mm thick, 7.6 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763 |
Ineos ABS Lustran® 356 Extrusion, Low-Gloss
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Impact Test | 31.0 J @Thickness 2.50 mm |
22.9 ft-lb @Thickness 0.0984 in |
Instrumented Impact, Total Energy; 2.5 mm thick, 7.6 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763 |
Ineos ABS Lustran® 552 Extrusion, Profile/Substrate Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Impact Test | 31.0 J | 22.9 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON DX93500 PC LNP STAT-KON* DX93500 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Impact Test | 31.0 J | 22.9 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON MD000IS PP LNP STAT-KON* MD000IS is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Impact Test | 31.0 J @Temperature 5.00 °C |
22.9 ft-lb @Temperature 41.0 °F |
Montell drop weight impact strength |
LyondellBasell Pro-fax SV258 Polypropylene Impact Copolymer Key Features: good impact and stiffness balance, good cold impact resistance, excellent dimensional stability, FDA acceptableApplications: corrugated board extrusion, appliancesMeets FDA requirement.. |
|||
Impact Test | 31.0 J | 22.9 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Impact Test | 31.0 J | 22.9 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |
|||
Impact Test | 31.0 J | 22.9 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific) LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |