Polymer Property : Impact Test = 237 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 237 J

@Thickness 6.35 mm,
Temperature -40.0 °C
175 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
Impact Strength; Max Force; ARM
ExxonMobil Escorene® LL-8461 LMDPE Rotational Molding Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.LL-8400 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8461 is fully formu..
Impact Test 237 J

@Thickness 6.35 mm,
Temperature -40.0 °C
175 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
Impact Strength; Max Force; ARM
ExxonMobil Escorene® HD-8660 LHDPE Rotational Molding Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8660 is fully formula..
Impact Test 237 J

@Thickness 6.35 mm,
Temperature -40.0 °C
175 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
Impact Strength; Max Force; ARM
ExxonMobil Escorene® HD-8661 LHDPE Rotational Molding Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8661 is fully formula..
Impact Test 237 J

@Thickness 6.35 mm,
Temperature -40.0 °C
175 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
Impact Strength; Max Force; ARM
ExxonMobil Escorene® LL-8556 LMDPE Rotational Molding Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A linear medium density polyethylene having improved flow characteristics vs. LL-8300's series resins, yet retaining outstanding whiteness and a goo..
Copyright © lookpolymers.com All Rights Reserved