Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 20.5 J | 15.1 ft-lb | multiaxial, at 2.2 m/sec, 100% ductile; ASTM 3763 |
S&E Specialty Polymers TufFillâ„¢ 5004UV Polyolefin Application: Thermoplastic polyolefin material is designed for molded in color automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV p.. |