Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 2.96 J | 2.18 ft-lb | Multi-Axial Instrumented Impact Energy; ISO 6603-2 |
LNP Thermocomp® GF-1006 Polysulfone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |