Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 2.30 J | 1.70 ft-lb | Multi-Axial Instrumented Impact Energy; ISO 6603-2 |
LNP Thermocomp® UC-1006 Polyphthalamide, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Impact Test | 2.30 J | 1.70 ft-lb | Multi-Axial Instrumented Impact Energy; ISO 6603-2 |
LNP Stat-Kon® LC-1003 Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |