Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 125 J | 92.2 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Impact Test | 125 J | 92.2 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Impact Test | 125 J | 92.2 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Impact Test | 125 J | 92.2 ft-lb | RT. 450°C tempering temp. Specimen size: 7x10x55 mm unnotched. Hardened at 960°C. Quenched in air. Tempered twice |
Assab Steels CARMO Cold Work Steel CARMO is a high-strength, flame-induction and through hardening steel delivered prehardened to 240-270 HB.The surface of the steel can be flame-hardened without water cooling to a hardness of 58±2.. |